| specific gravity | 2.6~2.8g/cm³ | bend strength | >300kg |
| hardness | >9 MOH′S | Tensile strength | >150kg/cm³ |
| porosity rate | <30% | Radiancy | 0.85 |
| atmosphere | Furnace Temperature(ºC) | Surface Load(W/cm2) | The influence on the Rod |
| Ammonia | 1290 | 3.8 | The action on SiC produces methane and destroys the protection film of SiO2 |
| Carbon dioxide | 1450 | 3.1 | Corrode SiC |
| Carbon monoxide | 1370 | 3.8 | Absorb carbon powder and influence the protection film of SiO2 |
| Halogen | 704 | 3.8 | Corrode SiC and destroy the protection film of SiO2 |
| Hydrogen | 1290 | 3.1 | The action on SiC produces methane and destroys the protection film of SiO2 |
| Nitrogen | 1370 | 3.1 | The action on SiC produces insulating layer of silicon nitride |
| Sodium | 1310 | 3.8 | Corrode SiC |
| silicon dioxide | 1310 | 3.8 | Corrode SiC |
| Oxygen | 1310 | 3.8 | SiC oxidized |
| Water-vapor | 1090-1370 | 3.1-3.6 | The action on SiC produces hydrate of silicon |
| Hydrocarbon | 1370 | 3.1 | Absorb carbon powder resulted in Hot pollution |


![]() ![]() |
![]() ![]() |